Help! I have a question concerning the use of anode baskets in place of
anode bars. What are the advantages and disadvantages of using anode
baskets? Which shape of basket is better, round or rectangular? Does any
one out there have any technical data available?
You can reach me at Details Inc. (714)-630-4077
Paul Walker
Sr. Process Eng.
|
|
|