TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipchq.com (Smail3.1.28.1 #2) id m0sm6kc-0000GpC; Fri, 25 Aug 95 16:57 CDT
Old-Return-Path:
<miso!hou.sperry-sun.com!DDrake_at_SSDSRDCC>
Date:
Fri, 25 Aug 1995 16:21:49 -0500
Precedence:
list
X-Loop:
Resent-Sender:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/959
TO:
Return-Path:
Resent-Message-ID:
<"FryKB2.0.y57.-SaFm"@ipc>
Subject:
From:
Resent-From:
From [log in to unmask] Sat Apr 27 14:
38:48 1996
Message-Id:
Parts/Attachments:
text/plain (19 lines)
     
     We are having a lot of problems with soldering tip erosion while using 
     high temperature solders (typically 221 deg.C Eutectic and 300 deg.C 
     MP). Realizing that most tips are Copper core iron-clad, tin or 
     tin/lead plating.
      
     Typical fluxes are RMA and some with OA.
       
     Does anyone have suggestions and or recommendations on where we can 
     locate soldering tips that have less erosion factor and is wettable ? 
     Or where we can have some made ?
     
     Darrell Drake
     Sr. Process Engineer
     DRAKE@SSDSRDCC
     (713) 987-4365