Mime-Version: |
1.0 |
Content-Type: |
TEXT/PLAIN; CHARSET=US-ASCII |
Old-Return-Path: |
<miso!uunet.uu.net!fluke!barum> |
Date: |
Fri, 25 Aug 1995 07:46:45 DST |
Precedence: |
list |
Reply-To: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
Priority: |
Normal |
Content-Length: |
992 |
TO: |
|
Return-Path: |
|
Resent-Sender: |
|
X-Loop: |
|
X-Mailing-List: |
|
Resent-Message-ID: |
<"LVdh13.0.WCC.MKUFm"@ipc> |
Subject: |
|
From: |
|
Resent-From: |
|
Received: |
by ipchq.com (Smail3.1.28.1 #2)
id m0sm0DH-0000GlC; Fri, 25 Aug 95 09:58 CDT |
From [log in to unmask] Sat Apr 27 14: |
38:20 1996 |
Message-Id: |
|
Parts/Attachments: |
|
|
On Thu, 24 Aug 1995 13:22:08 -0700 Glynn Shaw wrote:
> From: Glynn Shaw <[log in to unmask]>
> Date: Thu, 24 Aug 1995 13:22:08 -0700
> Subject: Source for Peelable Mask
> To: [log in to unmask]
>
> Looking to acquire peelable mask made by a German company named Lockwerke
> Peters.
> Have no other information. Anybody use this stuff or know where to get it?
>
> Thanks in advance,
> G. Shaw
> Proto Engineering
> Sunnyvale, Ca.
> fax: (408) 738-0693
>
Glynn:The material your looking for is probably SD 2954.There are a
couple of other products for specialty applications in their 2800
series.I "think" the Ca. distrubutor is C.I.S. Phn# 714 288 4247 if
not call Lackwerke Peters GmbH direct at 02152 2009 0.