Mime-Version: |
1.0 |
Content-Type: |
TEXT/PLAIN; CHARSET=US-ASCII |
Old-Return-Path: |
<miso!telecomm.tadiran.co.il!mickey> |
Date: |
Wed, 26 Jul 1995 08:30:53 +0300 (IDT) |
Precedence: |
list |
Reply-To: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
|
Resent-Sender: |
|
X-Loop: |
|
Resent-From: |
|
Received: |
by ipchq.com (Smail3.1.28.1 #2)
id m0sb6zS-0000H4C; Wed, 26 Jul 95 08:59 CDT |
Resent-Message-ID: |
<"SMSjT1.0.0k6.gea5m"@ipc> |
Subject: |
|
From: |
|
Sender: |
|
In-Reply-To: |
|
From [log in to unmask] Sat Apr 27 14: |
25:40 1996 |
Message-Id: |
<Pine.3.05.9507260832.A4155-b100000@neptune> |
Parts/Attachments: |
|
|
hi tom,
A reference which we keep using as a guide is found in mil-f-14072b,
para. 3.13 and the table of "compatible couples".
There are also solderability issues associated with gold plated lugs.
regards,
mickey
On Thu, 20 Jul 1995, Tom Tindale wrote:
> We have a customer who requires tin/tin type sockets as opposed to tin/gold
> for all their socketed components. Their reasoning is based on the corrosion
> potential from the dissimilar metals. Our problem is that tin/tin sockets
> are becoming increasingly more difficult to obtain, and in some cases more
> expensive than their gold plated counterparts. My question is: Has anyone
> have any information or done any testing on this subject. We would like to
> change their thinking if possible. Any information would be appreciated.
>
> Thanks,
>
> Thomas Tindale
> Lead Manufacturing Engineer
> Performance Computer
> 315 Science Parkway
> Rochester, New York 14620
> 716.256.0200 Phone
> 716.256.0791 Fax
> e-mail [log in to unmask]
>
|
|
|