We have a big problem with Solder Bridging on our Bottom Side SMT
components in Wave Solder. These are Glued on at SMT then Waved in
Wave Solder. We have tried everything under the Sun and have
eliminated most of the Bridges but not all. Any suggestions.
ERic Bernal at Pragmatech, Sunnyvale, Ca
(408)734-0595
[log in to unmask]
|
|
|