TECHNET Archives

March 2024

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 20 Mar 2024 14:54:29 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (214 lines)
Hi Joyce,

I see that nobody got the post I made earlier either. I can only
communicate by replying to the sparse emails that show up once in a blue
moon.

I've contacted the IPC and the IPC answers desk via email, but they don't
seem to want to be bothered with the Technet list anymore.

I find that strange because the listserver still keeps a history of
anything you post, it's just not sending it out to all of the members:

https://linkprotect.cudasvc.com/url?a=http%3a%2f%2flistserv.ipc.org%2fscripts%2fwa.exe%3fA1%3dind2403%26L%3dTECHNET%26X%3dOA7ABD561BF127A026B%26Y%3dsgregory%2540kimco.net&c=E,1,utptAhaahnaPvUVJLR_ma13_7CvTbhtHGOwBQ80J1sAA1enSMjAmaWiENIZPhaK93NioKAmSjJbOWHaLzrXYdhQ-Bij-zZM8iKroXZABn6x5&typo=1

It's too bad, I found over the years that Technet is a very valuable
resource. I guess they don't care anymore

Steve

On Wed, Mar 20, 2024 at 2:30 PM Joyce Koo <
[log in to unmask]> wrote:

> I didn't.
> jk ;-(
> > I got it Steve.
> >
> > Ioan
> >
> > De : Steve Gregory <[log in to unmask]>
> > Envoyé : March 20, 2024 8:49 AM
> > À : TechNet E-Mail Forum <[log in to unmask]>; Ioan Tempea
> > <[log in to unmask]>
> > Objet : Re: [TN] Surface energy for conformal coating
> >
> > Hi all,
> >
> > So I've seen Doug's reply and Ioan's reply. I'm going to reply and see if
> > anybody gets this...
> >
> > Steve
> >
> > On Wed, Mar 20, 2024 at 6:34 AM Ioan Tempea
> > <[log in to unmask]<mailto:
> [log in to unmask]>>
> > wrote:
> > Thanks Doug,
> >
> > Can't get it more thorough than that!
> >
> > We do have a Surface Analyst so I guess I'll request a side by side
> > dyne/contact angle characterization, to get the angle equivalents of 40+
> > dynes.
> >
> > Best regards,
> >
> > Ioan
> >
> > -----Message d'origine-----
> > De : TechNet <[log in to unmask]<mailto:[log in to unmask]>> De la part de
> > Pauls, Doug O Collins
> > Envoyé : March 20, 2024 8:18 AM
> > À : [log in to unmask]<mailto:[log in to unmask]>
> > Objet : Re: [TN] Surface energy for conformal coating
> >
> > You're welcome.
> >
> > Indiscrete Answers
> > - We will typically take surface energy readings when we qualify a new
> > board site, then monitor a few incoming lots, but often we do not test
> > again unless we have reason to go looking.  The dyne pens, while
> > inexpensive and easy to use, are variable in interpretation.  A more
> > accurate and repeatable measurement can be made with instruments designed
> > to measure surface tension and surface energy.  There is one by Kruss,
> out
> > of Switzerland, and one from Brighton Science (formerly BTG Labs)
> (Surface
> > Analyst).  We have both.  Both work.
> > -  Yes, manufacturing processes can impact surface energy.  When we
> > qualify a site, we have a qualification vehicle fabricated by the
> > candidate site that then goes through our manufacturing processes.  Then
> > we measure surface energy to see how much the manufacturing process
> > impacted the surface.  We  have some very robust cleaning processes, so
> we
> > seldom see the surface energy go down if the solder mask was fully cured
> > to start with.
> >
> > Douglas Pauls | Sr. Technical Fellow | Electronics AMT COLLINS AEROSPACE
> > 400 Collins Road NE, MS 108-101, Cedar Rapids, IA  52498  USA
> > Tel: +1 319 295 2109 | Mobile: +1 319 431 3773
> >
> > -----Original Message-----
> > From: TechNet <[log in to unmask]<mailto:[log in to unmask]>> On Behalf Of
> Ioan
> > Tempea
> > Sent: Wednesday, March 13, 2024 6:11 AM
> > To: [log in to unmask]<mailto:[log in to unmask]>
> > Subject: [External] Re: [TN] Surface energy for conformal coating
> >
> > Thanks Doug!
> >
> > Indiscreet questions:
> > - How do you make sure your spec is what you get? Do you request dyne
> > testing by the PCB fab?
> > - Do you measure dynes at Incoming or just in case you have issues on the
> > assembly line?
> > - Does surface energy variate during assembly? I mean a 40+ dynes/cm at
> > Incoming, will it stay the same after 2 reflows, some TH assembly,
> rework,
> > staking, etc., even with proper cleaning?
> >
> > Best regards,
> >
> > Ioan
> >
> > -----Message d'origine-----
> > De : TechNet <[log in to unmask]<mailto:[log in to unmask]>> De la part de
> > Pauls, Doug Collins Envoyé : March 12, 2024 10:03 PM À :
> > [log in to unmask]<mailto:[log in to unmask]> Objet : Re: [TN] Surface energy
> > for conformal coating
> >
> > Ioan,
> > In general, I have used this rule of thumb:
> > <30 dynes/cm - you will see problems with adhesion and wetting.
> > 30-35 dynes/cm - you will still see problems with adhesion and wetting,
> > but not as much as under 30.
> > 35-40 dynes/cm - generally decent adhesion and wetting but occasional
> > issues
> > 40+ dynes/cm - good adhesion and wetting.  Collins specifies >44 dynes/cm
> > for its solder mask.
> >
> > Douglas Pauls | Sr. Technical Fellow | Electronics AMT COLLINS AEROSPACE
> > 400 Collins Road NE, MS 108-101, Cedar Rapids, IA  52498  USA
> > Tel: +1 319 295 2109 | Mobile: +1 319 431 3773
> >
> > -----Original Message-----
> > From: TechNet <[log in to unmask]<mailto:[log in to unmask]>> On Behalf Of
> Ioan
> > Tempea
> > Sent: Monday, March 11, 2024 2:42 PM
> > To: [log in to unmask]<mailto:[log in to unmask]>
> > Subject: [External] [TN] Surface energy for conformal coating
> >
> > Hello Technos,
> >
> > Some many years ago I have discovered, with help from this illustrious
> > panel, the existence of the dyne pens. Have used them for a while and
> them
> > moved to microelectronics, where I have spent 11 years without any
> contact
> > with conformal coating. So I've kinda forgot some details.
> > Where I work we have the Surface Analyst device, measuring contact angles
> > and this is supposed to obsolete the use of dyne pens.
> >
> > The trouble is I can't remember what dyne values are related to good
> > coating wetting. Or even better, which contact angles are preferred?
> >
> > Can anyone help?
> > I'm interested in both solder masked PCBs and Au plated ceramics and the
> > optimal values I believe differ from PCB to ceramics.
> >
> > Also, do you have any good articles or textbooks to recommend on this
> > matter?
> >
> > Thanks,
> >
> > Ioan
> >
> >
> > --
> > Steve Gregory
> > Kimco Design and Manufacturing
> > Process Engineer
> > (208) 322-0500 Ext. -3133
> > Cell Phone: (918) 706-2779
> >
> > [
> https://linkprotect.cudasvc.com/url?a=https%3a%2f%2fkimco.net%2fEmailLogos%2fKDMsig200.png&c=E,1,0APBNUk0JMqSWmGtbQ-2dgP4NS89V7fk5PB3LC6-K_ea5qcPK8EohtSXRw3aowB6LulGdhRY0tALvdEN2gAJdwTx4K7DstOXuQCKkuHbu349PYjoZg,,&typo=1
> ]
> > This email and any attachments are only for use by the intended
> > recipient(s) and may contain legally privileged, confidential,
> proprietary
> > or otherwise private information. Any unauthorized use, reproduction,
> > dissemination, distribution or other disclosure of the contents of this
> > e-mail or its attachments is strictly prohibited. If you have received
> > this email in error, please notify the sender immediately and delete the
> > original.
> >
>


-- 
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
Cell Phone: (918) 706-2779

-- 


This email and any attachments are only 
for use by the intended 
recipient(s) and may contain legally privileged,
 confidential, proprietary 
or otherwise private information. Any 
unauthorized use, reproduction, 
dissemination, distribution or other 
disclosure of the contents of this 
e-mail or its attachments is strictly
 prohibited. If you have received 
this email in error, please notify the
 sender immediately and delete the 
original. 

ATOM RSS1 RSS2