https://linkprotect.cudasvc.com/url?a=https%3a%2f%2fcaswellplating.com%2felectroplating-anodizing%2fblack-nickel-plating-kits.html&c=E,1,I31Qez8ufHcaOnEnoVNzucVsfMbjLZUA-mYc5aiD_7yDrbQWi94DpPPmBqYSSwKCELfUHEFn0VFTqsdrqYlFdUUGojqibdPxSEw36VPDMQ,,&typo=1 No personal experience with nickel, but some used their tin plate to create tin whiskers. On Tue, Feb 22, 2022 at 9:35 AM Hernandez, Victor G < [log in to unmask]> wrote: > Fellow TechNetters: > Many, many, many moon ago Buehler LTD offered a Nickel Plating kit, > Pre-Clean, Solution A&B Kit, for Back Plating Nickel. > This product is currently discontinued with no replacement product, > Does anyone out there have any recommendations for a substituted > product/vendor. > > Victor, > -- Denny Fritz Consultant 812 584 2687