TECHNET Archives

May 2021

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 4 May 2021 12:50:41 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Yes Agreed. 

Potting is even a better choice.



Rich  Kraszewski 





* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *

This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls

Sent: Monday, May 3, 2021 4:56 PM

To: [log in to unmask]

Subject: Re: [TN] [External] Re: [TN] TechNet archives? looking for information on coating or encapsulation long term protection



<html><body><p style="background-color:#F5AD7C; border:1px solid black;">[EXTERNAL] Use caution when clicking links or attachments from unknown senders.</p><br></body></html> Don't know Rich.  Sounds like he is looking more for a potting material.

---

*Douglas Pauls *| Technical Fellow | Electronics AMT



*COLLINS AEROSPACE*



400 Collins Road NE, MS 108-101, Cedar Rapids, IA  52498  USA



*Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773



[log in to unmask]



[log in to unmask] for all Export Compliant Items





On Mon, May 3, 2021 at 4:52 PM Richard Kraszewski < [log in to unmask]> wrote:



> I will that a guess that the coating you are looking for is likely 

> parylene, or possibly a silicone  coating.

>

> Rich  Kraszewski

> Plexus

>

> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * * This e-mail and 

> any attachments are confidential from Plexus Corp. and may contain 

> information which is privileged, confidential, and/or protected by 

> non-disclosure agreements.  They are intended solely for the use of 

> the named addressee(s).  .  Any unauthorized use or disclosure may be 

> unlawful.  If you are not a named addressee, you must not use, 

> disclose, retain or reproduce all or any part of the information 

> contained in this e-mail or any attachments If you have received this 

> transmission in error, please destroy it and notify us immediately by 

> return e-mail or by calling

> + 1 888 208 9005.

>

> -----Original Message-----

> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Hatano

> Sent: Monday, May 3, 2021 11:58 AM

> To: [log in to unmask]

> Subject: Re: [TN] TechNet archives? looking for information on coating 

> or encapsulation long term protection

>

> <html><body><p style="background-color:#F5AD7C; border:1px solid 

> black;">[EXTERNAL] Use caution when clicking links or attachments from 

> unknown senders.</p><br></body></html> Excellent!!!

> Thanks so much Steve.

> I hope you have a great day!

>

> Richard Hatano

> EDA Manager

>

> 3855 Ruffin Road, San Diego, CA 92123-1813  USA Direct  858-285-2392  

> | Fax  858-836-3400 [log in to unmask]

>

>

> -----Original Message-----

> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory

> Sent: Monday, May 3, 2021 9:56 AM

> To: [log in to unmask]

> Subject: Re: [TN] TechNet archives? looking for information on coating 

> or encapsulation long term protection

>

> EXTERNAL SENDER – Exercise Caution.

>

>

>

> Hi Richard,

>

> It's still there, check out:

> https://ddei5-0-ctp.trendmicro.com:443/wis/clicktime/v1/query?url=http

> s%3a%2f%2furldefense.com%2fv3%2f%5f%5fhttps%3a%2f%2fddei5%2d0%2dctp.tr

> endmicro.com%3a443%2fwis%2fclicktime%2fv1%2fquery%3furl%3dhttps%2a3a%2

> a2f%2a2flinkprotect.cudasvc.com%2a2furl%2a3fa%2a3dhttp%2a253a%2a252f%2

> a252flistserv.ipc.org%2a252fscripts%2a252fwa.exe%2a253fINDEX%2a26c%2a3

> dE%2a2c1%2a2c%2a2d%2a5fjKsmkPzskGmh426O6bq8UU5N5sxYZ8e0MOY0D1SPtmrYUHQ

> wzmiQGij5%2a5fWcIr%2a5fNtyKbi4kVnCsYNz0wRb4i5NIsOGttWtHS4XSD5kovZnBv8S

> fgrWHI3l4%2a26typo%2a3d1%26umid%3dE6764D8F%2dC16F%2dE005%2d9F9E%2d165A

> B66417E9%26auth%3dfa0282dc3c44b189bcc708f19c936975d8469bfe%2d553ee3487

> 38739e35723801315099f645a03cc41%5f%5f%3bJSUlJSUlJSUlJSUlJSUlJSUlJSUlJQ

> %21%21MvWE%21VIfdjJP8qX%2dnpQY%2dAPqU1vxX8G2bS9Fro3BnE%5fY8QPmrzarqhgG

> eWwxLlwkZ8YjqBQ%24&umid=A48E7829-C174-0705-8E4D-18D4D584F493&auth=fa02

> 82dc3c44b189bcc708f19c936975d8469bfe-93521325a05f21120d94d331f5d3669fa

> 7e482e7

>

> Steve

>

> On Mon, May 3, 2021 at 10:52 AM Richard Hatano 

> <[log in to unmask]

> >

> wrote:

>

> > Hi,

> >

> > Sorry to trouble, but I just discovered that the IPC homepage no 

> > longer seems to have a link to the online forum archives (maybe I 

> > haven't checked in quite a while!).

> > Are they now behind a registration wall?

> > I was looking for information on best encapsulants (coatings aren't 

> > looking capable) to provide 100 year protection to passive circuitry 

> > that will be buried approx. 3-8 ft. underground inside a 

> > polypropylene

> enclosure.

> > I hope everyone is doing well and send thanks if anyone can help 

> > point me in the right direction.

> >

> > Richard Hatano

> > EDA Manager

> > [logo]

> > 3855 Ruffin Road, San Diego, CA 92123-1813  USA Direct  858-285-2392

> > |  Fax  858-836-3400

> > [log in to unmask]<mailto:[log in to unmask]>

> >

>

>

> --

> Steve Gregory

> Kimco Design and Manufacturing

> Process Engineer

> (208) 322-0500 Ext. -3133

> Cell Phone: (918) 706-2779

>

> --

>

>

>

> This email and any attachments are only for use by the intended

> recipient(s) and may contain legally privileged,  confidential, 

> proprietary or otherwise private information. Any unauthorized use, 

> reproduction, dissemination, distribution or other disclosure of the 

> contents of this e-mail or its attachments is strictly  prohibited. If 

> you have received this email in error, please notify the  sender 

> immediately and delete the original.

>

> <p></p>

>



<p></p>


ATOM RSS1 RSS2