TECHNET Archives

May 2021

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Hernandez, Victor G" <[log in to unmask]>
Date:
Thu, 27 May 2021 14:04:12 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Larry Brophy <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
Never had a problem with it Victor.

Regards,

Larry

-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Hernandez, Victor G
Sent: Thursday 27 May 2021 14:03
To: [log in to unmask]
Subject: [TN] ENIG plating Flex Circuit

Fellow TechNetters:

   Is ENIG surface plating finish suitable for a flexible circuit in a Rigid
Flex application?   Nickel is brittle.