Yes. It works.
________________________________
From: Steve Gregory <[log in to unmask]>
Date: 11 February 2021 at 4:56:31 AM SGT
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] RTV Encapsulation of circuit boards
Hi Phil,
See if this link works: https://tinyurl.com/1p1rxi3m
Steve
On Wed, Feb 10, 2021 at 1:43 PM Nutting, Phil <[log in to unmask]>
wrote:
> Steve,
>
>
>
> Here is what I encountered.
>
> This site is blocked due to content filtering.
>
> Sorry, photos.google.com has been blocked by your network administrator.
>
> Sigh!
>
> Phil Nutting | Senior Development Engineer | Lab: +1-978-224-4334 *|*
> Mobile: +1-978-828-8664
>
> 35 Congress Street *|* Salem, MA 01970 *|* U.S.A. *|* *www.excelitas.com*
> <http://www.excelitas.com/>
>
>
>
>
>
>
>
> *From:* Steve Gregory <[log in to unmask]>
> *Sent:* Wednesday, February 10, 2021 3:40 PM
> *To:* TechNet E-Mail Forum <[log in to unmask]>; Nutting, Phil <
> [log in to unmask]>
> *Subject:* Re: [TN] RTV Encapsulation of circuit boards
>
>
>
> *EXTERNAL EMAIL:* Use caution with replies, links and attachments.
>
>
>
> Hi Phil,
>
>
>
> We don't use RTV but we do encapsulate a printed circuit assembly in a
> box. It's a mixed technology assembly with SMT and through hole. This
> assembly is a relay board that goes into vehicle HVAC systems, (ie: farm
> equipment, construction equipment, trucking) that we pot with a 2-part
> polyurethane compound from Epic Resins called their S7144. Here's a photo
> of a failed one that I cut the top of the case of a failed relay just to
> look and see what I could see. I'll see if this google image works:
> https://photos.app.goo.gl/oQvHwCbEm9TBFYvn9
>
>
>
> Steve
>
>
>
> On Wed, Feb 10, 2021 at 1:14 PM Nutting, Phil <[log in to unmask]>
> wrote:
>
> Technetters,
>
> We build several power supplies that use RTV in place of dielectric oil
> for our high voltage multipliers. The RTV allows us to get the same output
> level in a smaller package than a similar design using the dielectric oil
> as the insulator. The proper process is to medial blast (lightly) the
> circuit boards, prime them and then encapsulate the boards in the RTV.
> Both the media blasting and priming can be very subjective processes. And
> both have process issues in our manufacturing group. Simply eliminating the
> media blasting and priming is not a solution as the RTV will not bond to
> the boards and ultimately creating the potential for arcing to ground.
>
> Ideally potting a small box makes a disposable assembly, so the bonding
> quality and thermal size change of the RTV is not an issue. We use between
> 20 and 100 pounds of RTV per potted assembly. Disposal or repair of failed
> units is expensive.
>
> I am looking for folks that use RTV for encapsulation and what they use
> for a process to ensure good bonding between the RTV and circuit boards.
>
> Phil Nutting | Senior Development Engineer | Lab: +1-978-224-4334 |
> Mobile: +1-978-828-8664
> 35 Congress Street | Salem, MA 01970 | U.S.A. | www.excelitas.com<<http://www.excelitas.com<>
> http://www.excelitas.com/>
>
> [cid:[log in to unmask]]
>
>
>
>
> --
>
> Steve Gregory
>
> Kimco Design and Manufacturing
>
> Process Engineer
>
> (208) 322-0500 Ext. -3133
>
> Cell Phone: (918) 706-2779
>
>
>
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
Cell Phone: (918) 706-2779
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|