TECHNET Archives

August 2020

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v753.1)
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Date:
Thu, 27 Aug 2020 12:15:55 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII; delsp=yes; format=flowed
Parts/Attachments:
text/plain (24 lines)
Many thx.
jk
On Aug 27, 2020, at 11:38 AM, David Hillman wrote:

> Hi Joyce - the underplating is typically nickel.
>
> Dave Hillman
> Collins Aerospace
>
> On Thu, Aug 27, 2020 at 10:20 AM Yuan-chia Joyce Koo  
> <[log in to unmask]>
> wrote:
>
>> Gurus,
>> what is the std plating surface finishing  of ferrous metal
>> components leads?  Cu or Ni underlying layer (thickness X-micron)
>> with solderable surface for lead free? (98% Tin for example, assume
>> flash gold is too expansive  - >2000 per oz, shish).  Anything in the
>> field  that is new?  Is standard change from MIL to ASTM  for the
>> plating?  Many thanks.
>> regards,
>> jk
>>