Hi All,
We have these Cree Blue LED's (PN# CLM3A-BKW-CTBVA463) that keep sticking
to the $%$#&@
pick and place nozzle. We have a MY-19 and have tried changing timing,
nozzle diameters with no luck. We place an amber LED of the same series
that we have no problems with except for one or two once in a while.
I've tried dabbing a little Freecote mold release compound on the tip of
the nozzle, and now I'm putting the reel into a 170F oven to see if baking
them for a couple hours will help.
Does anybody have any other ideas that might help?
Steve Gregory
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|
|
|