TECHNET Archives

August 2020

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 5 Aug 2020 14:02:06 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (119 lines)
Hi All,

Just wanted to let everyone know that we ordered a 500-piece strip from
Mouser with the hopes that they would come from a different lot, and then
we could see if it was lot related, or something about the LED itself.

Ran the LED's from Mouser without a single error or mispick. So there was
some issue with the silicone lens with the particular reel from yesterday
that we couldn't machine place.

As a side note, Cree has yet to respond to my customer support request for
the issue. Sad part is I don't expect them to. Money talks, and we're just
a small fish in a big ocean...

Steve

On Wed, Aug 5, 2020 at 12:34 PM Robert Kondner <[log in to unmask]>
wrote:

> Larry,
>
>  I kind of recall the MyData machines having a pressure profile for parts.
> It can generate a "Blow Off" pressure that should release the parts. I
> recall setting it too high can blow around small passives.
>
> Bob K.
>
> -----Original Message-----
> From: TechNet <[log in to unmask]> On Behalf Of Davis, Larry
> Sent: Tuesday, August 4, 2020 3:36 PM
> To: [log in to unmask]
> Subject: Re: [TN] Cree Blue LED (PN# CLM3A-BKW-CTBVA463) Sticking to
> Nozzle...
>
> Hi Steve,
>
> We are not running Mycronic machines but switching to a plastic nozzle did
> correct this issue for us.
>
> Good luck,
>
> LARRY DAVIS | PCBA Production Engineer
> P 970.663.1377 ext 2774
> Hach Company | www.hach.com | [log in to unmask]
>
>
> -----Original Message-----
> From: TechNet <[log in to unmask]> On Behalf Of Steve Gregory
> Sent: Tuesday, August 04, 2020 12:21 PM
> To: [log in to unmask]
> Subject: [TN] Cree Blue LED (PN# CLM3A-BKW-CTBVA463) Sticking to Nozzle...
>
> Hi All,
>
> We have these Cree Blue LED's (PN# CLM3A-BKW-CTBVA463) that keep sticking
> to the $%$#&@ pick and place nozzle. We have a MY-19 and have tried
> changing timing, nozzle diameters with no luck. We place an amber LED of
> the same series that we have no problems with except for one or two once in
> a while.
>
> I've tried dabbing a little Freecote mold release compound on the tip of
> the nozzle, and now I'm putting the reel into a 170F oven to see if baking
> them for a couple hours will help.
>
> Does anybody have any other ideas that might help?
>
> Steve Gregory
>
> --
> Steve Gregory
> Kimco Design and Manufacturing
> Process Engineer
> (208) 322-0500 Ext. -3133
>
> --
>
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged,  confidential,
> proprietary or otherwise private information. Any unauthorized use,
> reproduction, dissemination, distribution or other disclosure of the
> contents of this e-mail or its attachments is strictly  prohibited. If you
> have received this email in error, please notify the  sender immediately
> and delete the original.
> Please be advised that this email may contain confidential information. If
> you are not the intended recipient, please notify us by email by replying
> to the sender and delete this message. The sender disclaims that the
> content of this email constitutes an offer to enter into, or the acceptance
> of, any agreement; provided that the foregoing does not invalidate the
> binding effect of any digital or other electronic reproduction of a manual
> signature that is included in any attachment.
>


-- 
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133

-- 



This email and any attachments are only 
for use by the intended 
recipient(s) and may contain legally privileged,
 confidential, proprietary 
or otherwise private information. Any 
unauthorized use, reproduction, 
dissemination, distribution or other 
disclosure of the contents of this 
e-mail or its attachments is strictly
 prohibited. If you have received 
this email in error, please notify the
 sender immediately and delete the 
original. 

ATOM RSS1 RSS2