TECHNET Archives

August 2020

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Davis, Larry" <[log in to unmask]>
Date:
Wed, 5 Aug 2020 14:34:22 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (53 lines)
Larry,

 I kind of recall the MyData machines having a pressure profile for parts. It can generate a "Blow Off" pressure that should release the parts. I recall setting it too high can blow around small passives.

Bob K.

-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Davis, Larry
Sent: Tuesday, August 4, 2020 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Cree Blue LED (PN# CLM3A-BKW-CTBVA463) Sticking to Nozzle...

Hi Steve,

We are not running Mycronic machines but switching to a plastic nozzle did correct this issue for us.

Good luck,

LARRY DAVIS | PCBA Production Engineer
P 970.663.1377 ext 2774
Hach Company | www.hach.com | [log in to unmask]


-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Steve Gregory
Sent: Tuesday, August 04, 2020 12:21 PM
To: [log in to unmask]
Subject: [TN] Cree Blue LED (PN# CLM3A-BKW-CTBVA463) Sticking to Nozzle...

Hi All,

We have these Cree Blue LED's (PN# CLM3A-BKW-CTBVA463) that keep sticking to the $%$#&@ pick and place nozzle. We have a MY-19 and have tried changing timing, nozzle diameters with no luck. We place an amber LED of the same series that we have no problems with except for one or two once in a while.

I've tried dabbing a little Freecote mold release compound on the tip of the nozzle, and now I'm putting the reel into a 170F oven to see if baking them for a couple hours will help.

Does anybody have any other ideas that might help?

Steve Gregory

--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133

--



This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged,  confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly  prohibited. If you have received this email in error, please notify the  sender immediately and delete the original.
Please be advised that this email may contain confidential information. If you are not the intended recipient, please notify us by email by replying to the sender and delete this message. The sender disclaims that the content of this email constitutes an offer to enter into, or the acceptance of, any agreement; provided that the foregoing does not invalidate the binding effect of any digital or other electronic reproduction of a manual signature that is included in any attachment.

ATOM RSS1 RSS2