As an FYI - David Hillman/Rockwell Collins wrote that paper.
Rich Kraszewski
Senior Staff Process Engineer
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, December 19, 2019 8:59 AM
To: [log in to unmask]
Subject: Re: [TN] LF Solder Bars, SN96.5AG3.0CU0.5, SAC305
[EXTERNAL] This email was sent from outside of Plexus. Use caution when opening attachments or links from unknown senders.
.
TechNetters,
Why would ANY solder (with the possible exception of solder preforms that were flux encrusted) have an expiration date? I seem to recall there being a paper where someone did rework with solder wire with flux in it that was
20 years old and there was no problem.
Regards,
Bev
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of [log in to unmask]
Sent: Thursday, December 19, 2019 9:27 AM
To: [log in to unmask]
Subject: [TN] LF Solder Bars, SN96.5AG3.0CU0.5, SAC305
Fellow TechNetters:
Does Solid Bar LF Solder Vaculoy have an associated EXPIRATION DATE?
Victor,
|
|
|