TECHNET Archives

August 2019

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 30 Aug 2019 09:14:34 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Schaefer <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
Dave Schaefer <[log in to unmask]>
Parts/Attachments:
text/plain (12 lines)
Robert,

From Amitron website:

" Non-Conductive fill has a thermal conductivity of 0.25 W/mK whereas Conductive pastes have a thermal conductivity anywhere from 3.5-15 W/mK. In contrast, electroplated copper has a thermal conductivity of more than 250W/mK.

So while Conductive via fill can offer needed conductivity in some applications more often than not it is possible to use non-conductive paste and add additional vias. Often this results in superior thermal and electrical conductivity with minimal cost impact. "

Recall reading a more complete paper on this somewhere but can't locate it right now.

More ammunition for the idea of using many smaller VII non-conductively filled vias and calling out increased minimum hole plating (Class 3 hole plating).