TECHNET Archives

August 2019

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 26 Aug 2019 10:26:39 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tan Geok Ang <[log in to unmask]>
Message-ID:
Subject:
From:
Tan Geok Ang <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (18 lines)
no. it should not be flipped over for another 10sec. But we do specified suppliers to dip it twice or even 3rd time. depends on our requirements

________________________________

From: [log in to unmask] <[log in to unmask]>
Date: 26 August 2019 at 6:19:41 PM SGT
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] TM-650 2.6.8, Thermal Stress, Plated Through Holes.

Fellow TechNetters:

   Requesting clarification on the above stated TM.

   Section 5.6  Using tongs, carefully remove the test specimen from the solder and place it on a piece of insulator to cool to room temperature ( see 6.3).