TECHNET Archives

March 2019

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D
Date:
Tue, 5 Mar 2019 18:38:56 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
What type of component is it?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gil Zilber MTH
Sent: Tuesday, March 05, 2019 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] [External] [TN] SnAg component finish with SnPb solder past

Hi dave,
It is 1-3% silver.
Thanks.
Gil


-------- הודעה מקורית --------
מאת: David Hillman <[log in to unmask]>
תאריך: 4.3.2019 23:12 (GMT+02:00)
אל: TechNet E-Mail Forum <[log in to unmask]>, Gil Zilber MTH <[log in to unmask]>
נושא: Re: [External] [TN] SnAg component finish with SnPb solder past

Hi Gil - what is the composition of the SnAg plating?

Dave Hillman
Collins Aerospace
[log in to unmask]<mailto:[log in to unmask]>

On Mon, Mar 4, 2019 at 9:23 AM Gil Zilber MTH <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Hello,
Does anyone know if there is an issue of soldering components that have SnAg finish with SnPb solder paste?

Thanks,
Gil Zilber
Process Engineer at IAI

*********************************************************************************************** Please consider the environment before printing this email ! The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addressee thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer. Thank you. Visit us at: https://urldefense.proofpoint.com/v2/url?u=http-3A__www.iai.co.il&d=DwIFAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=1EcAWfE8N3tV5N8R-_vKcpyy81cpdr0C9ZtM2gH9g5I&s=78ShPh3PR8932eqz4gIGKUdnQNtQMVLLQmZgbjmSi08&e=

Default Profile 60
*********************************************************************************************** Please consider the environment before printing this email ! The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addressee thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer. Thank you. Visit us at: www.iai.co.il

ATOM RSS1 RSS2