Yes! https://www.accudynetest.com/adtpen.html
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Mary Davis
Sent: Tuesday, March 26, 2019 2:51 PM
To: [log in to unmask]
Subject: Re: [TN] [External] [TN] Conformal Coating & PCB Solder Resist Finish
Simple Accu dyne marking pens can be used to characterize the surface energy. Below 35 dyne/cm, adhesion is marginal to poor. Search the Technetium archives for "solder mask surface tension for conformal coating adhesion" 2014
Get Outlook for iOS<https://aka.ms/o0ukef> ________________________________
From: TechNet <[log in to unmask]> on behalf of Douglas Pauls <[log in to unmask]>
Sent: Tuesday, March 26, 2019 7:32:23 AM
To: [log in to unmask]
Subject: Re: [TN] [External] [TN] Conformal Coating & PCB Solder Resist Finish
Mark,
I would tend to agree that matte is better for that reason, but it can also be related to the surface energy of the mask.
*Douglas Pauls *| Principal Materials and Process Engr | Advanced Operations Engineering
*COLLINS AEROSPACE*
400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
*Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
[log in to unmask]
On Tue, Mar 26, 2019 at 8:55 AM Mark Austin <[log in to unmask]>
wrote:
> Hello
>
>
>
> Does anyone have any experience of applying conformal coatings to
> different PCB Solder Resist finishes? I am thinking that matt finish
> solder resist would promote better wetting of the conformal coating,
> and possibly better long-term adhesion.
>
>
>
> Best Regards
>
>
>
> Mark Austin
>
> Lead Engineer
>
>
>
> D +44 (0) 1329 242325
>
> T +44 (0) 845 658 6111
>
> F +44 (0) 845 658 6222
>
> <
> https://urldefense.proofpoint.com/v2/url?u=http-3A__www.phoenixsystems
> uk.com_&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=lTRDjB8ojaf7ZaJ9DHeDAm7e-H
> FP9fxIkv6fRnV49HE&m=90GOMT2e_v8DvYt3WEn4TR-utfEvMCSsYLqIySgvlxA&s=oHuQ
> 1tVdijPszpFiDTWeDFyR9tK7OQOE2ZBCyWb05NU&e=>
>
> https://urldefense.proofpoint.com/v2/url?u=http-3A__www.phoenixsystems
> uk.com&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=lTRDjB8ojaf7ZaJ9DHeDAm7e-HF
> P9fxIkv6fRnV49HE&m=90GOMT2e_v8DvYt3WEn4TR-utfEvMCSsYLqIySgvlxA&s=8pJ1y
> Nm98ZSBPV-2CQux4EjOG4GaoMOl8E9DRUZ2W3w&e=
>
>
>
> P Please consider your environmental responsibility, do you really
> need to print this e-mail?
>
> Registered Office: Unit 48, Standard Way, Fareham
> Industrial Park, Fareham, Hants. PO16 8XQ.
>
> Registered in England & Wales, Number 4356233
>
>
>
|
|
|