This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
-----Original Message-----
From: Stadem, Richard D [mailto:[log in to unmask]]
Sent: Friday, March 1, 2019 5:31 AM
To: TechNet E-Mail Forum <[log in to unmask]>; Richard Kraszewski <[log in to unmask]>
Subject: RE: [TN] [External] [TN] Table comparing benefit/drawbacks of Conformal Coating versus Potting
[EXTERNAL] This email was sent from outside of Plexus. Use caution when opening attachments or links from unknown senders.
.
Rich,
Here is a good paper on the subject.
https://www.electrolube.com/technical-articles/conformal-coatings-vs-potting-compounds-which-is-better-to-protect-my-pcb-a-coating-or-a-resin/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Thursday, February 28, 2019 8:51 PM
To: [log in to unmask]
Subject: Re: [TN] [External] [TN] Table comparing benefit/drawbacks of Conformal Coating versus Potting
Many thanks for the quick reply & details Doug.
I already have the section you were referring to.
Rich Kraszewski
Senior Staff Process Engineer
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Thursday, February 28, 2019 10:23 AM
To: TechNet E-Mail Forum <[log in to unmask]>; Richard Kraszewski <[log in to unmask]>
Subject: Re: [External] [TN] Table comparing benefit/drawbacks of Conformal Coating versus Potting
[EXTERNAL] This email was sent from outside of Plexus. Use caution when opening attachments or links from unknown senders.
.
Rich,
There is no such table in IPC-HDBK-850 on potting. There is a section in IPC-HDBK-830A that is titled "Conformal coating vs. Potting and Encapsulation". This is just text and not a table. Is that what you are looking for? If so, I can send that section to you.
Douglas Pauls | Principal Materials and Process Engr | Advanced Operations Engineering COLLINS AEROSPACE
400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
Tel: +1 319 295 2109 | Mobile: +1 319 431 3773 [log in to unmask]<http://collins.com>
On Thu, Feb 28, 2019 at 10:06 AM Richard Kraszewski <[log in to unmask]<mailto:[log in to unmask]>> wrote:
I seem to recall a table such as this may already exist. Somewhere in IPC documents or industry presentations .
If anyone recalls such a table and its location is readily handy, I would appreciate a copy.
Would save me the time to recreate.
Thanks in advance .
Rich Kraszewski
Senior Staff Process Engineer
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|