These are parameters you should determine by testing. I am retired now but remember requiring re-priming if >30 hours had elapsed. It is also my memory that poor adhesion results if vapor deposited primer is applied to existing Parylene coating - while acceptable adhesion is obtained when liquid applied primer is applied over existing Parylene. Again, you should do some testing on your processes to establish acceptable practices.
Good luck,
Mary Davis
Retired Materials and Process Engineer
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Richard Kraszewski
Sent: Saturday, January 5, 2019 9:15 AM
To: [log in to unmask]
Subject: [TN] Hey Coating Techies
Two parylene coating related questions regarding primers:
#1 - What is the maximum time you would allow between priming and depositing the parylene?
#2 - I have been lead to believe that if you place primer on an already coated parylene surface , the primer will act as a release agent for the next layer of parylene. Better not to add primer in this case but rather recoat ASAP. Would welcome any and all thoughts.
Thanks in advance
Rich Kraszewski
Senior Staff Process Engineer
Plexus
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|