TECHNET Archives

January 2019

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Mary Davis <[log in to unmask]>, "Douglas Pauls ([log in to unmask])" <[log in to unmask]>
Date:
Tue, 29 Jan 2019 13:39:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D" <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (33 lines)
Yes, Mary, you are just like me. I remembered the paper spot test from my days in electronics kindergarten so I tried googling it up and found quite a good bit of information on it. It was called sulfur acetate paper.
Here is just one: https://www.canada.ca/en/conservation-institute/services/conservation-preservation-publications/canadian-conservation-institute-notes/test-sulfur-acetate-paper.html


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mary Davis
Sent: Monday, January 28, 2019 1:32 PM
To: [log in to unmask]
Subject: Re: [TN] Recommendation for Sulfur Spot Tests

I can't give you anything but a vague memory.  It is my memory that decades ago glass slides with a vapor deposited silver mirror coating were used to test paper packaging materials for the presence of sulfur.  Sulfur caused the silver mirror to turn black.  Sorry I don't have any more details.

Mary Davis, 
Retired Materials & Process Engineer

-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Richard Kraszewski
Sent: Monday, January 28, 2019 10:30 AM
To: [log in to unmask]
Subject: [TN] Recommendation for Sulfur Spot Tests

Anyone aware of a good spot test  to quickly check  for sulfur (sulphur) which they are willing to share??

Currently, using the iodine-azide method from the classic Organic Spot Test book by Feigl with limited success. 
Hoping some else could recommend some other. 

Rich  Kraszewski 
Senior Staff Process Engineer

* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *

This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.