Hi Steve,
I just bought one not too long ago for our stockroom for the same purpose.
Quincy Labs, PN# 31-350. You can buy a brand new bench-top oven with a
18-month warranty, decent inside chamber dimensions of 25.5" x 30" x 24"
.for $1863.00. UPS shipping to Boise was $257.61. I wanted a good sized
chamber for multiple 13" reels,
Steve
On Thu, Nov 15, 2018 at 12:23 PM Vargas, Stephen M <
[log in to unmask]> wrote:
> Good afternoon:
>
> I am looking for an economical oven that will allow us to bake
> moisture sensitive parts at a low temperature (40 degrees C, </= 5% RH).
> This is for SMT parts that are not conducive to placing in a high
> temperature oven due to package considerations (T&R, etc.). Offline
> responses welcome. Thanks in advance.
>
> Regards,
> Steve Vargas
>
> If you don't have time to do it right, when will you have time to do it
> over?
> John Wooden
>
> Lockheed Martin RMS-Rotary and Mission Systems
> Polaris Contract Mfg.
> 15 Barnabas Rd
> Marion, MA 02738
> 774-553-6192
> [log in to unmask]<mailto:[log in to unmask]>
>
> P Please consider the environment before printing this e-mail
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|