The usual alternative to silicone adhesive is acrylic adhesive. I tried
eliminating silicone adhesives years ago when I was running a plating
operation. The experiment failed dismally:
-There was no evidence the silicone ever caused a problem with de-wetting
or other issues silicone OILS cause--so I did this based on principal as
opposed to practicality!
-Silicone adhesive for tapes stick best to other silicone, so after you
peel, there is usually no residue at all
-Acrylic adhesives drop little globs of acrylic all over the place. The
worst offender is the half-sticky stuff such as "Post-It" notes.
Wayne Thayer
On Wed, Oct 3, 2018 at 7:06 AM Vargas, Stephen M <[log in to unmask]>
wrote:
> Good morning all:
>
> We are looking to move away from silicone based adhesives with our
> Kapton tape to a non-silicone based version. It appears as though 3M has a
> 7419 Series that may be a good option. I'm looking for input from those of
> you who have switched and would like some recommendation on what has worked
> well for you. Off-line responses welcome. Thanks.
>
> Regards,
> Steve Vargas
>
> If you don't have time to do it right, when will you have time to do it
> over?
> John Wooden
>
> Polaris Contract Mfg Inc
> 15 Barnabas Rd
> Marion, MA 02738
> 774-553-6192
> [log in to unmask]<mailto:[log in to unmask]>
>
> P Please consider the environment before printing this e-mail
>
|
|
|