Fellow TechNetters:
Besides black bees wax, has anyone out there has experience with adhesives (Super Glue) for mounting SMT VR packages (0.1120 x 0.0730 inch) and/or silicon, IC, onto a cross section fixture. Currently I have been using Super Glue Liquid. However, my SMT package keeps falling off the fixture holder. All comments and suggestions are welcomed.
Victor,