Hi Victor,
That's a pretty iffy looking mounting hole, and to tell you the truth, that
kind of damage doesn't surprise me. There was a flat washer beneath that
screwhead wasn't there?
http://stevezeva.homestead.com/PTH_Diameter_vx_Screw_Head_Overlap.pptx
Steve
On Fri, Aug 17, 2018 at 8:54 AM, <[log in to unmask]> wrote:
> Fellow TechNetters:
>
> I am searching for hardware mounting selection guidelines for the
> purpose of avoiding future damage to PWB PTH external copper pad by
> retaining screw head.
>
> Example pics and current dimensions have been sent to Steve Gregory,
> [log in to unmask]<mailto:[log in to unmask]>
>
>
>
> Givens:
>
> - PWB PTH Slot Diameter, 138.450 mm
>
> - Screw Head Diameter, 159.640 mm
>
> - Screw Shank Diameter, 87.740 mm
>
> - Potential mating overlap, 21.190 mm
>
>
>
> Victor,
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|