Hi Rob,
Although this is not NIST traceable, I've made a Go-No/Go gage at the end
of our inspectors little 6" stainless steel ruler. I used a Dremel and cut
a little 2.5mm notch at the end that they can use as a Go-NoGo gage to
check the lead length. I did use a set of Calipers to check the depth of
the notch and they are calibrated. The inspectors love it.
http://stevezeva.homestead.com/Lead_Length_Go-NoGo.jpg
Steve
On Wed, Aug 8, 2018 at 10:43 AM, Robert Coburn <
[log in to unmask]> wrote:
> Hi T-netters;
> The Company just certified to AS9100.
> One of the minor observations related to the method used to measure the
> lead length to insure compliance with IPC requirements.
> Are there any tools/devices/equipment available to measure lead lengths
> that is repeatable/traceable and will fulfill the AS9100 requirement?
> I look forward to your responses.
> Regards,
> Rob
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged,
confidential, proprietary
or otherwise private information. Any
unauthorized use, reproduction,
dissemination, distribution or other
disclosure of the contents of this
e-mail or its attachments is strictly
prohibited. If you have received
this email in error, please notify the
sender immediately and delete the
original.
|
|
|