There are many labs that offer X-ray or CT scans, along with microsectioning, etc. For a one-time or for occasional requirements they are great.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Thursday, August 30, 2018 1:26 PM
To: [log in to unmask]
Subject: [TN] qualifying a heatsink attach process
Hi technet!
We've got a customer working with high power transistors, they want to
use solder pre-forms to solder a heatsink on top of a row of
transistors. So the stackup will be PCB - transistor - preform -
heatsink, where the heatsink will span a row of 5 transistors.
The question is how do we establish that this is working OK and isn't
full of voids? This is at the "ok, we think this will work but we need
to qualify the attachment method" stage. I've come up with a couple of
options:
1) tear / grind it off and look for anomalies - not very sure to find
issues.
2) x-ray it - we don't have a 3-d x-ray so I'm not confident in our
abilities to find voiding. We do have a nice static x-ray though and
will try it to see how well it can see.
3) Sonoscan it to look for voids? Would have to be outsourced.
Am I missing any obvious options?
--