Hi Todd,
Thanks for your reply.
I'm keen to try the magnetic option, having seen it first hand and now knowing others have had success. I'm unsure though if we have enough clamping area to work with, and if the step will affect printing of the uBGA's.
Can I ask, why you used a nonmagnetic metal? I had been thinking of a stainless steel shim which would simplify the foil design.
I presume you included cut-outs in your carrier to align/mate with the foil attached magnets so as not to add height to your step?
What was this thickness of your foil?
Did you follow IPC 7525's design rules on keep-out for a Step-Down stencil of 0.9 mm for every 0.025 mm of step-down thickness?
Daragh OLoughlin
Lead NPI Engineer
Cochlear Limited
12 Helen Street
Newstead QLD 4006
AUSTRALIA
Phone: +61736346775
Email: [log in to unmask]
www.cochlear.com
-----Original Message-----
From: MacFadden, Todd [mailto:[log in to unmask]]
Sent: Thursday, 5 July 2018 11:09 PM
To: TechNet E-Mail Forum <[log in to unmask]>; Daragh OLoughlin <[log in to unmask]>
Subject: RE: Screen Printing on 0.4 mm +/-0.1 thick PCB's
Hi Daragh,
We have had good success with the magnetic hold down approach you mention. We use aluminum sheets that cover the entire circuit array with cutouts only at the SMT areas (we epoxy magnets on the underside of the Al sheets that align with opposite-polarity magnets embedded in corresponding holes in the fiberglass carriers). This works really well to keep the flex circuits flat during stenciling and pick-and-place.
Todd MacFadden
Component Reliability Engineer
BOSE
Technology Centers of Excellence
Materials Engineering and Analysis
Office: +1 508.766.6259
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Daragh OLoughlin
Sent: Thursday, July 5, 2018 7:06 AM
To: [log in to unmask]
Subject: [TN] Screen Printing on 0.4 mm +/-0.1 thick PCB's
Hi All,
I'm looking for advice from anyone with experience printing to thin Flex-Rigid Polyimide-based PCB's. I'm interested in suggestions/tips for carrier retention mechanisms/designs and/or Screen Print tooling support of PCB's of 0.4 mm +/-0.1 thickness.
As far as carrier design concepts, with a 0.4mm thin board, using low height tooling pins to date do not provide adequate retention/support. We have also tried various spring systems in the carrier to provide tension through the tooling pins to the board in X/Y directions to assist the retention, but to date no concept was worked well. Additionally, our carrier supplier recommended a high friction coating applied to carriers, however this coating degrades with use and has a limited life, and it's not a preferred option. I have personally visited a large manufacturing site in China, and saw them use magnets inserted into holes bored in the underside of the carrier, epoxy sealed in place, and use a thin metal foil overlay (with a large window with ~5mm clamping area on each side of the panel) to provide X, Y and Z retention.
Does anyone have any suggestions for a robust carrier design suitable? Or perhaps can recommend a supplier to contact?
Product Info:
Flex-Rigid Polyimide-based PCB is panelised – width 69mm, length 128 mm Finished PCB thickness: 0.4 mm +/-0.1 mm There are two fine pitch BGA components located 3mm from the panel edges (both clamping sides)
Pitch: 0.4 mm and 0.35 mm
Bump diameter: nominal 0.130 mm
Pad Diameter: 0.2 mm
Manufacturing equipment
DEK Horizon 03iX Screen printer
DEK Horizon 02i Screen Printer
Stencil Info:
0.0762mm (~0.003”) Laser Cut Electro-polished Stencil
Daragh OLoughlin
Lead NPI Engineer
Cochlear Limited
12 Helen Street
Newstead QLD 4006
AUSTRALIA
Phone: +61736346775
Email: [log in to unmask]
www.cochlear.com
==============================================
"The information contained in this e-mail message may be confidential information, and may also be privileged. If you are not the intended recipient, any use, interference with, disclosure or copying of this material is unauthorised and prohibited. If you have received this message in error, please notify us by return email and delete the original message."
==============================================
"The information contained in this e-mail message may be confidential information, and may also be privileged. If you are not the intended recipient, any use, interference with, disclosure or copying of this material is unauthorised and prohibited. If you have received this message in error, please notify us by return email and delete the original message."
|