We appreciate your input also, Ekaterina! I think many of us learned something important about coating strippers. So thanks!
Odin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ekaterina Stees
Sent: Tuesday, July 17, 2018 2:53 PM
To: [log in to unmask]
Subject: Re: [TN] Urethane Coat Remover
Doug, it's for localized rework. Just looking into alternatives to potentially corrosive KOH.
Technetters, I appreciate everyone's input!