TECHNET Archives

July 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 17 Jul 2018 19:04:39 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Issue is the it is potentially as bad as applying  a very acidic flux  and taking a risk that it will all not be washed off afterwards. 

Caustic can be very unforgiving (corrosive & conductive) if not removed.

~ Like using oven cleaner on the assembly. 



Rich  Kraszewski 

Senior Staff Process Engineer

Plexus 





* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *



This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D

Sent: Tuesday, July 17, 2018 1:28 PM

To: [log in to unmask]

Subject: Re: [TN] Urethane Coat Remover



Pardon my ignorance, but what is the issue with the stripper having potassium hydroxide in it?



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory

Sent: Tuesday, July 17, 2018 11:55 AM

To: [log in to unmask]

Subject: Re: [TN] Urethane Coat Remover



Hi Kate,



Stripping Urethane coating as you know is very difficult to strip. If you

have a stripper that works well on the urethane, you then have to be

careful whether or not it will affect any other material on the assembly. I

found one that doesn't have potassium hydroxide in it. I've never used it,

so I don't know how well it works:



https://www.miller-stephenson.com/product/conformal-coating-stripper/



These are the ingredients:



Material

CAS No.                    Approx. %

1,1,1,2,2,3,4,5,5,5-Decafluoropentane (HFC-43-10mee)

138495-42-8               22 - 30%

Trans,1.2-Dichloroethylene

156-60-5                     45 - 50%

Methanol

67-56-1                       4 - 10%

N-Methyl-2-Pyrrolidone

872-50-4                     18 - 22%



When we had a big project where we had to rework a bunch of boards that

were urethane coated, it was an engineering change where we had to remove

and replace parts on boards that were urethane coated we purchased a

micro-abrasion station from a company called CCR Co.



http://www.ccrco.com/



I think I remember it being recommended by a Lockheed engineer. Anyways the

station worked great. The media used in the station is ESD safe which is

something you need to worry about when using a media-blasting station.

Urethane is best stripped when it is aged a bit. When it is freshly applied

the beads tend to bounce off. I remember if they didn't strip well I would

put them into an oven for a few hours to make the coating become a little

harder so it would strip easier.



Steve



On Tue, Jul 17, 2018 at 5:45 AM, Ekaterina Stees <[log in to unmask]>

wrote:



> Hello Technetters,

> Does anyone know of a chemical remover for urethane conformal coat that

> does not use potassium hydroxide as it's active ingredient?

>

> Thanks,

> Kate

>







-- 

Steve Gregory

Kimco Design and Manufacturing

Process Engineer

(208) 322-0500 Ext. -3133



-- 







This email and any attachments are only 

for use by the intended 

recipient(s) and may contain legally privileged,

 confidential, proprietary 

or otherwise private information. Any 

unauthorized use, reproduction, 

dissemination, distribution or other 

disclosure of the contents of this 

e-mail or its attachments is strictly

 prohibited. If you have received 

this email in error, please notify the

 sender immediately and delete the 

original. 


ATOM RSS1 RSS2