TECHNET Archives

July 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ekaterina Stees <[log in to unmask]>
Date:
Tue, 17 Jul 2018 10:54:52 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (77 lines)
Hi Kate,

Stripping Urethane coating as you know is very difficult to strip. If you
have a stripper that works well on the urethane, you then have to be
careful whether or not it will affect any other material on the assembly. I
found one that doesn't have potassium hydroxide in it. I've never used it,
so I don't know how well it works:

https://www.miller-stephenson.com/product/conformal-coating-stripper/

These are the ingredients:

Material
CAS No.                    Approx. %
1,1,1,2,2,3,4,5,5,5-Decafluoropentane (HFC-43-10mee)
138495-42-8               22 - 30%
Trans,1.2-Dichloroethylene
156-60-5                     45 - 50%
Methanol
67-56-1                       4 - 10%
N-Methyl-2-Pyrrolidone
872-50-4                     18 - 22%

When we had a big project where we had to rework a bunch of boards that
were urethane coated, it was an engineering change where we had to remove
and replace parts on boards that were urethane coated we purchased a
micro-abrasion station from a company called CCR Co.

http://www.ccrco.com/

I think I remember it being recommended by a Lockheed engineer. Anyways the
station worked great. The media used in the station is ESD safe which is
something you need to worry about when using a media-blasting station.
Urethane is best stripped when it is aged a bit. When it is freshly applied
the beads tend to bounce off. I remember if they didn't strip well I would
put them into an oven for a few hours to make the coating become a little
harder so it would strip easier.

Steve

On Tue, Jul 17, 2018 at 5:45 AM, Ekaterina Stees <[log in to unmask]>
wrote:

> Hello Technetters,
> Does anyone know of a chemical remover for urethane conformal coat that
> does not use potassium hydroxide as it's active ingredient?
>
> Thanks,
> Kate
>



-- 
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133

-- 



This email and any attachments are only 
for use by the intended 
recipient(s) and may contain legally privileged,
 confidential, proprietary 
or otherwise private information. Any 
unauthorized use, reproduction, 
dissemination, distribution or other 
disclosure of the contents of this 
e-mail or its attachments is strictly
 prohibited. If you have received 
this email in error, please notify the
 sender immediately and delete the 
original. 

ATOM RSS1 RSS2