TECHNET Archives

May 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Frank Kimmey <[log in to unmask]>
Date:
Wed, 16 May 2018 17:33:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (43 lines)
there are literature in the past regarding the mechanical stress  
distribution of LGA vs BGA... yes, increase solder paste will help  
somewhat, but you should minimize the smily or use the corner  
adhesive if necessary... check Cisco paper many years ago regarding  
the corner adhesive for large BGA (where you get your BGA from? if   
it is from large vendor, not repackaged stuff, you should ask for  
thermorie data (check thermoire google search, it may pop out many  
papers regarding size, BGA stand offs, and FEM),  and compare  to  
your own reflow profile and  see if you use it outside their  
recommended reflow profile... most likely, it is)..
best of luck.
jk
On May 16, 2018, at 5:12 PM, Frank Kimmey wrote:

> Can anyone point me in a good direction to learn more about  
> solderjoint elasticity with SAC305.
> We are seeing some issues with BGAs when they smile.
> Type 2 fractures and the vendor recommends increasing the solderpaste.
> This seems counter intuitive to me.
> If it was SnPb I would go back and hunt some of Werner's research.
> As it is Lead free I need some direction.
> Any help is appreciated,
> FNK
>
> Frank N Kimmey CID+
> Electrical Engineer/PCB Design
>
> Verifone
> 1400 W Stanford Ranch Road
> Rocklin, CA 95765
> T: 916-625-1818
> M: 916-833-9877
>
> *********************************************************
> This electronic message and any attachments are intended only for  
> the use of the addressee. The information in this electronic  
> message is confidential and proprietary, and may include privileged  
> information. If you are not the intended recipient, please delete  
> this electronic message and any attachments and notify the sender  
> of the error. Please be aware that any unauthorized use,  
> dissemination, distribution or copying of this message or any  
> attachments is strictly prohibited.

ATOM RSS1 RSS2