We updated our conformal coating programs (selective spray) to avoid our 2D barcodes, both label and laser engraved. I didn't investigate other barcode scanners at the time as it seemed easier to modify our programs than to buy a bunch of new scanners. For 2D matrix barcodes in general, I've had good success with a Zebra DS4308 XD. But I don't know if it would work well through coating.
Thanks,
Ryan Elson
Manufacturing Engineer
Bently Nevada
Baker Hughes, a GE company
Cell +1 775 790 5182
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: Tuesday, May 08, 2018 2:20 PM
To: [log in to unmask]
Subject: EXT: [TN] Barcode scanners through conformal coating
We are printing 2D Aztec barcodes on Brady thermal transfer labels made out of polyimide material and applying these onto our circuit assemblies.
We then apply conformal coat (Humiseal 1B73 or 1A33) on the assemblies and also the label. Our current barcode scanner, Zebra DS2208, cannot read the labels after coating.
What make and model of scanners are you using successfully for this situation?
Thanks
Peter
________________________________
The enclosed documents are proprietary items to Silicon Forest Electronics' (SFE) customers. They shall not be reproduced nor disclosed for any purpose except as specified in writing from an authorized agent of SFE. These documents may contain data restricted for export by the International Traffic in Arms Regulations (ITAR) section of the Arms Export Control Act (or the Export Administration Act). Violators are subject to severe criminal penalties.
This e-mail, and any file attached to it, is meant only for the intended recipient of the transmission and may be a communication privileged by law. If you have received it in error, please notify the sender immediately and delete the original from your system. Any other use of this e-mail by you is strictly forbidden.
|
|
|