Hello to all
We have problems with the time to baking Tape and Reel Packing, because is
very extensive time.
But we received a component that supplier recommended the baking according
IPC033 but also:
60°C 0+/5°C (100mbar). How the component is tape and reel is not possible
to use 24h@125°C so we need to use the second option.
Our doubt, are there guideline in the IPC about time with baking with vacuum
(around 100mbar), to we use that recommendation to others components with
tape and reel packing? Because, according to the supplier the time is
shorter, when this process is used.
Thank you
|
|
|