The Technet Forum stands waiting, and we jump and respond immediately to all of your requests and inquiries!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, April 03, 2018 10:40 AM
To: [log in to unmask]
Subject: Re: [TN] IPC Guideline for Gull Wing lead PWB pad to component lead ratio
Dell - Internal Use - Confidential
Thanks for sharing the information and for the prompt response time......
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 3, 2018 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] IPC Guideline for Gull Wing lead PWB pad to component lead ratio
IPC-SM-782, IPC-7351
On Tue, Apr 3, 2018 at 9:00 AM, <[log in to unmask]> wrote:
> Fellow TechNetters:
>
> Can someone point me in the right direction for PWB SMT pad dimensions
> for gull wing devices? Heel LF solder fillet formation concern.
>
> Victor,
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
|
|
|