I agree, I should have clarified the etchback issue.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Showers
Sent: Thursday, April 19, 2018 9:11 AM
To: [log in to unmask]
Subject: Re: [TN] R: [TN] R: [TN] PCB failure
The real problem is that this PCB has no etchback, positive or negative (PCBs are defective). As far as resin recession, yes the processing probably caused the separation, but once again, the PCB has no etchback.