np.
On Apr 6, 2018, at 9:51 AM, <[log in to unmask]>
<[log in to unmask]> wrote:
> Dell - Internal Use - Confidential
>
> Joyce,
>
> Thank you very much for your input/experience. Very
> enlightening.......
>
> Victor,
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Yuan-chia Joyce
> Koo
> Sent: Friday, April 6, 2018 8:19 AM
> To: [log in to unmask]
> Subject: Re: [TN] FW: IPC-A-610G, section 5.2.9,, Solder anomalies-
> Fractured solder, Defect 1, 2, 3 (Axial leaded device)
>
> as I said before, the 20% is not universal applicable. you need
> to have data to back up why it is 20%... (for smaller BGA, I would
> do 10% max). IMHO.
>
>
> On Apr 6, 2018, at 8:55 AM, <[log in to unmask]>
> <[log in to unmask]> wrote:
>
>> Dell - Internal Use - Confidential
>>
>> Joyce,
>>
>> Is there supported documentation for the Post Sequential Test
>> allowable percentage (20% max.)?
>>
>> Victor,
>>
>> -----Original Message-----
>> From: Yuan-chia Joyce Koo [mailto:[log in to unmask]]
>> Sent: Friday, April 6, 2018 7:43 AM
>> To: TechNet E-Mail Forum <[log in to unmask]>; Hernandez, Victor G
>> <[log in to unmask]>
>> Subject: Re: [TN] FW: IPC-A-610G, section 5.2.9,, Solder anomalies-
>> Fractured solder, Defect 1, 2, 3 (Axial leaded device)
>>
>> at time zero - as out of factory - no fracture allowed - if you have
>> fracture at BGA solder mask area, you got crack initiation site - you
>> need to change solder mask openning to avoid such a fault IMHO.
>>
>> At end of sequential test (vib, thermal shock, drop/impact), 20%
>> max.... Noted in qual report for review as item of susceptibility of
>> overall system design - program manager have to sign up for knowingly
>> accept the reliability risk.
>>
>> If it is go to sky or some places that repair and overhaul are not
>> allowed, you have to have redundancy exist to avoid potential failure
>> risk. 20% is based on electrical design and thermal design
>> requirements for device under overall assembly level design... not
>> cast in stone and not universal (23% was maximum based on FEM and
>> design assessment of worst case performance in this case to derive to
>> 20%, for example, max environmental temp plus assembly add on
>> operational temperature for signal current carrying capability and
>> thermal conduction capability - special attention to the power and
>> ground..etc.etc)... for example.
>> hopefully, it helps.
>> jk
>> On Apr 6, 2018, at 6:53 AM, <[log in to unmask]> wrote:
>>
>>> Fellow TechNetters:
>>>
>>> I was surprised that very little input was provided.
>>> Therefore, since it Friday Elements QUIZ day. I will take advantage
>>> of the high volume traffic day.
>>>
>>> Victor,
>>>
>>> From: Hernandez, Victor G
>>> Sent: Thursday, April 5, 2018 10:22 AM
>>> To: TechNet E-Mail Forum <[log in to unmask]>
>>> Cc: Hernandez, Victor G <[log in to unmask]>
>>> Subject: IPC-A-610G, section 5.2.9,, Solder anomalies-Fractured
>>> solder, Defect 1, 2, 3 (Axial leaded device)
>>>
>>> Fellow TechNetters:
>>>
>>> Is there a percentage associated with the statement "Fractured
>>> Solder" in the above stated IPC STD section?
>>> I did not a similar statement, Fractured Solder, for Surface Mount
>>> Devices and Surface Mount Area.
>>> Is there an acceptable percentage of the solder joint lead interface
>>> that can be fractured?
>>>
>>>
>>> Victor,
>>
|