Better to pre-tin the mildly oxidized parts, it may be a lot cheaper than changing your wash system to accommodate a new flux.
There are lots of "it depends" needed to answer that question.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jose A Rios
Sent: Thursday, April 26, 2018 12:06 PM
To: [log in to unmask]
Subject: [TN] Flux question
Is ROL0 flux an adequate one when faced with having to solder marginally oxidized components. Or should a different flux type be selected. Application is ground based/hi-rel (non flight). Flowdown is J-001 (not space addendum). Thanks….
José (Joey) Ríos, Sr QA Engineer
Mission Assurance Manager
Kavli Institute for Astrophysics & Space Research Massachusetts Institute of Technology [log in to unmask]<mailto:[log in to unmask]>