TECHNET Archives

April 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 13 Apr 2018 17:36:56 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Showers <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="utf-8"
Content-Transfer-Encoding:
quoted-printable
From:
Wayne Showers <[log in to unmask]>
Parts/Attachments:
text/plain (9 lines)
You might want to check out this paper:
Characteristic Times of Moisture Diffusion and Bake-out Conditions for Plastic Encapsulated Parts 
written by 
Alexander Teverovsky
QSS Group, Inc./Goddard Operations
[log in to unmask]

I have emailed you a copy.  Of note is that the key temperature for any bake out under vacuum is 58C.