TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Mon, 5 Mar 2018 17:38:14 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Decker, Scott UTAS" <[log in to unmask]>
Message-ID:
Subject:
From:
"Decker, Scott UTAS" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
OK, from yet another dinosaur to another, (I guess) that's what I thought you said too Jack... :-) :-)



On top of that, it has nothing to do with non-functional pads either!  Just saying...and also covering the next phase of questions before they get asked, just in case... :-) :-) 



Is it Monday already??? Oh man, it IS.....



Scott Decker – Staff Engineer, PCB Design Services CID+ – Electronic Systems Center

UTC AEROSPACE SYSTEMS

3445 S. 5th Street, Suite 170, Phoenix, AZ 85040 U.S.A.

Tel: 602 308 5957  FAX: 602 243 2347

KE7MWT  AKA:PadMasterson

[log in to unmask]   www.utcaerospacesystems.com



CONFIDENTIALITY WARNING: This message may contain proprietary and/or privileged information of

UTC Aerospace Systems and its affiliated companies. If you are not the intended recipient please 1) do not disclose, copy,

distribute or use this message or its contents, 2) advise the sender by return e-mail, and 3) delete all copies (including all

attachments) from your computer. Your cooperation is greatly appreciated.

This Document Does Not Contain Export Controlled Technology Or Technical Data.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson

Sent: Monday, March 05, 2018 10:12 AM

To: [log in to unmask]

Subject: [External] Re: [TN] Conformal Coating on Edge of CCA



I agree!

I meant to say that if the edges are conductive, they might need to be exposed (wait a minute... that IS what I said!)



thanks,

Jack



On Mon, Mar 5, 2018 at 10:18 AM, Douglas Pauls < [log in to unmask]> wrote:



> Well Jack, sometimes the board edges are metallized so that it serves 

> as a grounding path and sometimes as a thermal conduction path.  In 

> those cases, the presence of conformal coating interferes with the 

> function of the board and so it should not be present.  That is 

> usually the question I ask designers all the time - will conformal 

> coating in Location X interfere with the form, fit or function of the 

> unit.  If yes, then it is a keep out zone.

>

>

> Doug Pauls

> Principal Materials and Process Engineer Rockwell Collins

>

> On Mon, Mar 5, 2018 at 10:00 AM, Jack Olson <[log in to unmask]> wrote:

>

>> Typically the goal is to protect conductive surfaces, and board edges 

>> don't often have conductive surfaces (and if they do, they might need 

>> to stay exposed).

>>

>> If you have seen the board edges coated it is probably a result of 

>> the method that was used to coat them (spraying or dipping), not 

>> because it was required.

>>

>>

>>

>> On Thu, 1 Mar 2018 09:45:26 -0600, Caitlen Gahm < 

>> [log in to unmask]> wrote:

>>

>> >Greetings,

>> >

>> >We are wondering what the general thought is regarding whether or 

>> >not

>> the edge of a CCA/PWB needs to be conformally coated?  We received 

>> CCA's from a supplier and noticed that the edges were not coated.  

>> Our thinking thus far is that since our drawing does not state that 

>> coating on the edge is optional or not required, it would be required.

>> >

>> >What we are curious to know is what the general consensus is 

>> >regarding

>> whether or not it is necessary to coat the edge of the CCA and 

>> instances when this would or would not be desired.

>> >

>> >Thank you,

>> >Caitlen Gahm

>> >Materials and Process Engineer

>> >Crane Aerospace & Electronics

>>

>

>