Hi Guy,
That's the one big thing that I liked about the focused Infrared light
rework station that I used in the past, it was a PDR Lightmaster Pro. If
you didn't want to heat up adjacent components all you would have to do is
shield them with aluminum foil and reflect the light away from the area.
Steve
On Fri, Mar 30, 2018 at 2:18 PM, Guy Ramsey <[log in to unmask]> wrote:
> We are seeing more and more designs where it is not possible, with our BGA
> reworkstation, to remove or reinstall components and not reflow adjacent
> parts, or in some cases, part on the opposite side of the assembly.
> What action do you all take to mitigate the resulting conditions?
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
|
|
|