As I am the chair of the 7-11 Test Methods SC, let me state for the record
that our group is merely the gatekeeper for the TM-650 methods manual.
Methods are submitted by various task groups for our review and subsequent
adoption into the methods manual. Each of the methods have an originating
task group defined in the upper right hand corner of the method. Whoever is
defined in that section is the owner of a given method.
If I understand Victors question, he wants to know why the methods don't
reference a particular standard. The test methods only define a procedure
for how to conduct a specific test. Sometimes methods are called out or are
referenced by a standard, but not always. There are a lot of test methods
that aren't called out in IPC standards, but are still relevant for
evaluating different aspects of printed board and assembly production.
Methods themselves are not standards and therefore do not call out specific
pass / fail criteria. Usually such criteria, assuming a method is called
out in a spec, can only be found in the spec.
As to your specific method references below, you can find them here:
http://www.ipc.org/test-methods.aspx
2.1.1 is owned by 7-12 Microsectioning SC, the current chair of this group
is Russ Shepherd, NTS Anaheim
2.1.1.2A is a cancelled method because it either is no longer called in a
spec or the Originating Task Group requested it be cancelled. D-33a owns
this method.
2.6.8 is owned by D-33a Rigid Printed Board Performance TG, currently
co-chaired by Randy Reed, Reed Consultancy, LLC and Mark Buechner, BAE
Systems
I would encourage you to contact these gents if you have specific questions
/ concerns about the methods you reference. I know the men listed and
they're all good eggs and knowledgeable on the subject matter.
I hope this helps.
Best Regards,
Joe Russeau
Process Analyst
Precision Analytical Laboratory, Inc.
329 E. Firmin Street
Kokomo, IN 46902
P: (765) 252-3970
F: (765) 252-3971
C: (765) 210-0953
E: [log in to unmask]
Visit us on the web at www.precisionanalysts.com
-----Original Message-----
From: Stadem, Richard D
Sent: Thursday, March 08, 2018 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] TM-650-2.1.1; 2.1.1.2 & 2.6.8
Yes. On all standards, there is a committee listed. In the introduction.
For TM650, that group is identified as the Test Methods Subcommittee.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, March 08, 2018 8:50 AM
To: [log in to unmask]; Stadem, Richard D
Cc: [log in to unmask]
Subject: RE: [TN] TM-650-2.1.1; 2.1.1.2 & 2.6.8
Dell - Internal Use - Confidential
Richard,
Any idea who owns/responsible for TMs?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D
Sent: Thursday, March 8, 2018 8:31 AM
To: [log in to unmask]
Subject: Re: [TN] TM-650-2.1.1; 2.1.1.2 & 2.6.8
There is a form on the next to last page of every single IPC
standard........
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, March 08, 2018 7:53 AM
To: [log in to unmask]
Subject: Re: [TN] TM-650-2.1.1; 2.1.1.2 & 2.6.8
Well Victor, if Technet cannot answer your question, your next step would be
to pose the question to IPC Staff, such as John Perry, who is very involved
with the IPC-6012 and associated board efforts. He can then direct your
questions to the Leadership of A-600 for a response. That's what this old
dinosaur would do....
Doug Pauls
Principal Materials and Process Engineer Rockwell Collins
On Thu, Mar 8, 2018 at 7:49 AM, <[log in to unmask]> wrote:
> Fellow TechNetters:
>
> I did not receive responses to my initial inquiry. Therefore, I post
> once again. IMHO, Industry Standards are so convoluted that it takes a
> dinosaurs to interpret the documents much less draw correlation
> between the documents.
>
> Victor,
>
> From: Hernandez, Victor G
> Sent: Monday, March 5, 2018 12:37 PM
> To: 'TechNet E-Mail Forum' <[log in to unmask]>
> Cc: Hernandez, Victor G <[log in to unmask]>
> Subject: TM-650-2.1.1; 2.1.1.2 & 2.6.8
>
> Fellow TechNetters:
>
> What is the purpose of IPC-A-600 (J) if this standard document is
> not stated/mentioned/referenced in the above TMs.
> 2.1.1 section 5.4.3 Quality Observations,
> etc..............
> 2.1.1.2 section 5.2.3 Evaluation, etc..........
> 2.6.8 section 5.7.2 Examine for compliance,
> etc.......
>
> Is there a separate document for NEW Laminate Qualification.
>
> Victor,
>
---
This email has been checked for viruses by Avast antivirus software.