TECHNET Archives

January 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Mack <[log in to unmask]>
Date:
Wed, 10 Jan 2018 18:36:57 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, rkondner <[log in to unmask]>
Message-ID:
Subject:
From:
rkondner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=utf-8; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (15 lines)
Hi,

When we setup 2 selective Soldering machines the vendor strongly 
recommended higher purity, 99.99 or better.

Does anyone have experience with what level of purity is "Really" 
required? What does a user see as the purity drops?

Thanks,
Bob K.