TECHNET Archives

December 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, SALA GABRIELE <[log in to unmask]>
Date:
Fri, 1 Dec 2017 07:27:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (155 lines)
what I mean is the item (10) or similar to be present and covered  
with specific requirement for the application (see example  
listed...), as for 5G application in radar frequency, I am sure you  
can add few items, as for wirebondable gold, you might want purity  
spec more than MIL-std to ensure your yield.  As for MEMS, or any  
embedded, you might want to add few line as well (over pressure  
resulted fractured or damaged embedded may cost you great deal to FA,  
if one line dwg can resolve the issue... for example).   IMHO.   
(designer's pen should really gold plated...;-).
http://blog.epectec.com/creating-standard-pcb-fabrication-notes

On Dec 1, 2017, at 6:09 AM, SALA GABRIELE wrote:

> Inviato: venerdì 1 dicembre 2017 10:30
> A: 'TechNet E-Mail Forum'; 'Yuan-chia Joyce Koo'
> Oggetto: R: [TN] IPC Standard, bare board vendor markings
>
> HI
> As already stated by previous posts:
>
> IPC-6012 D   3.3.5  Marking... give useful guidelines  it recalls also
> IPC/J-STD-609 B also a very good guide lines similar (Joint Std) to  
> IEC
> 62588 Marking and Labeling, etc . BTW  the "driver" are always the  
> product
> and drawings specifications defined in the contract..
>
> Gabriele
> -----Messaggio originale-----
> Da: TechNet [mailto:[log in to unmask]] Per conto di Yuan-chia Joyce Koo
> Inviato: venerdì 1 dicembre 2017 01:50
> A: [log in to unmask]
> Oggetto: Re: [TN] IPC Standard, bare board vendor markings
>
> you should not standardize the note.  common usage- yes.  but not
> standardize - too many new requirements for new product...(5G is  
> comming).
> If you standardize the dwg note, there is no wirebondable gold come  
> out for
> example (all MIL std...).  IMHO.  So many hi-Rel product required  
> specific
> dwg notes, for example, chip on board, didn't have std dwg note  
> until almost
> 10-15 years later... (possibly still don't have std dwg note).
> jk
> On Nov 30, 2017, at 5:03 PM, Steve Golemme wrote:
>
>> All the notes are to supplement the standards.
>>
>> Have there been any efforts to standardize note options? I know it's
>> something I've done almost everywhere I've worked.
>>
>> Regards,
>> Stephen Golemme
>> Manufacturing Engineer
>> 650-214-5647
>> x.company
>>
>> On Thu, Nov 30, 2017 at 1:49 PM, Jose A Rios <[log in to unmask]> wrote:
>>
>>> Neither UL markings nor stackup markings are IPC requirements.
>>> Again go to
>>> 6012D section 3.3.5; its outlined there.
>>>
>>> Sent from my iPhone
>>>
>>> On Nov 30, 2017, at 4:11 PM, Stadem, Richard D <Richard.Stadem@GD-
>>> MS.COM< mailto:[log in to unmask]>> wrote:
>>>
>>> It doesn't necessarily have to be. Fabrication drawing notes, and
>>> notes on the assembly drawing normally take precedence over industry
>>> standards, as they are product-specific.
>>> The fab drawing and the assembly drawing are the "Bible" thou shalt
>>> go by if there is a conflict. The exception to the order of
>>> precedence is generally something in the contract.
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of
>>> [log in to unmask]<mailto:[log in to unmask]>
>>> Sent: Thursday, November 30, 2017 2:13 PM
>>> To: [log in to unmask]<mailto:[log in to unmask]>
>>> Subject: Re: [TN] IPC Standard, bare board vendor markings
>>>
>>> Dell - Internal Use - Confidential
>>>
>>> Is this statement supported (referenced) in an IPC/Industry  
>>> Standard?
>>>
>>> Victor,
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Golemme
>>> Sent: Thursday, November 30, 2017 2:07 PM
>>> To: [log in to unmask]<mailto:[log in to unmask]>
>>> Subject: Re: [TN] IPC Standard, bare board vendor markings
>>>
>>> We deal with power boards and sealing surfaces. The note I've had
>>> success with is:
>>>
>>> SUPPLIER SHALL MARK STACKUP AND DATE CODE, SUPPLIER NAME AND/OR
>>> TRADEMARK, AND UL FLAMMABILITY RATING IN NON-CONDUCTIVE INDELIBLE  
>>> INK
>>> (COLOR WHITE OR BLACK). SUPPLIER SHALL NOT ADD ANY TEXT OR  
>>> MARKING IN
>>> COPPER.
>>>
>>> Stephen Golemme
>>> Manufacturing Engineer, Makani
>>> 650-214-5647
>>> solveforx.com/makani<http://solveforx.com/makani>
>>>
>>> On Thu, Nov 30, 2017 at 11:56 AM, Jose A Rios  
>>> <[log in to unmask]<mailto:
>>> [log in to unmask]>> wrote:
>>>
>>> Silk screen (or etched metal) are acceptable forms of marking.
>>> Requirements for marking are basically legibility and traceability
>>> (you basically have to be able to match the conformance coupons to
>>> the boards they represent), by some method of serialization, which
>>> shall include date code. UL marking is not an IPC requirement, if
>>> required the board user must specify it. When using etched metal as
>>> marking, it shall not violate min spacing to board conductors (same
>>> with conductive inks). See 6012D 3.3.5 and its subsections.
>>>
>>>
>>> José (Joey) Ríos, Sr QA Engineer
>>> Mission Assurance Manager
>>> Kavli Institute for Astrophysics & Space Research Massachusetts
>>> Institute of Technology [log in to unmask]<mailto:[log in to unmask]>
>>> <mailto:
>>> [log in to unmask]>
>>> (617)324-6272
>>>
>>>
>>>
>>> On Nov 30, 2017, at 2:42 PM, [log in to unmask]<mailto:
>>> [log in to unmask]> wrote:
>>>
>>> Fellow TechNetters:
>>>
>>> IPC-1066 covers Lead free markings/Symbols/:Labels, etc.   Which IPC
>>> Standard covers bare board vendor logo/UL Rating/markings/production
>>> date/REV and layer counts.   Is silk screening printing of
>>> information
>>> acceptable beside etch from original external copper foil.
>>>
>>> Victor,
>>>
>
>
> ---