TECHNET Archives

November 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Gricel Guerrero-Gomez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gricel Guerrero-Gomez <[log in to unmask]>
Date:
Wed, 1 Nov 2017 15:38:56 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (17 lines)
Hello,

I received a batch of boards that show  what I would described as multiple nodules or "rough" surface all over the ENIG plated pads and mount holes. I have other batches where the surface looks smooth an even (no nodules). I would share a picture but I could not get to www.ipc.org/technet-photos.

I was trying to find anything related to these on IPC-6012 or IPC-4552 standards to see if this is acceptable.

What I found on the versions I have, is  that IPC-6012 only mentions for rectangular and round surface lands that any defect shall be maintained outside the pristine area, on the other hand a Wire Bond pad does mention a roughness requirement of 0.8*m RMS. All I found on IPC-4552 is that the surface shall be uniform.

Is there any requirement of roughness for the rectangular and round surface lands? Or, any specification on how big the nodules have to be to be considered a defect?

Thank you

Gricel Guerrero
Manufacturing Engineer
AJA Video Systems
(530) 271-3324