Richard,
If you intend to do power on testing of populated boards you must consider the type of coating (primarily the glass transition temperature) and coating coverage of leads with 90 degree edges plus under components, and pointed ends.
If your product is going to be used in a condensation type environment I strongly recommend you hermetically seal it. Remember water molecules are one of the smallest! What could occur is dendritic growth and intermittent shorts (worst case)!
David A. Douthit
Sent from my iPad
"
> On Nov 22, 2017, at 2:46 PM, Richard Kraszewski <[log in to unmask]> wrote:
>
> Other than what is written in IPC CC830 for thermal shock and MIR testing , is anyone away of any industry standard that addresses the functionality of coating or devices when exposed to condensation?
>
> I have looked at the IP Code for water ingress but all of that water testing seems too invasive & harsh for what I am looking for.
>
> https://en.wikipedia.org/wiki/IP_Code
>
> Something in IEC perhaps.
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|