TECHNET Archives

November 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 20 Nov 2017 13:23:02 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Message-ID:
Subject:
From:
Ioan Tempea <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Salut Eric,



You should start with this one http://flexiblecircuittechnology.com/flex4/



An important question : do you own the PCB design? You'll need to have a DfA say in all this!



For a good PCB design, all assembly is in the jigs, like Tan Geok said. You need to keep the flex portion rigid enough, even in the solder paste printer. Good fixture manufacturers (e.g. https://ascenteceng.com/, http://www.dmipallet.com/, http://www.emcgti.com/, http://www.pentagon-ems.com/ ) can give you priceless tooling design support.



Also, pre-assembly baking kinda becomes mandatory, polyimide is way more hygroscopic than FR4.



Regards,



Ioan Tempea, P. Eng.

Senior Manufacturing Engineer, Satellite Systems 



MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2

Tel: +1-514-457-2150 x3556

www.mdacorporation.com



This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.



-----Message d'origine-----

De : TechNet [mailto:[log in to unmask]] De la part de Eric Laroche

Envoyé : November 20, 2017 7:22 AM

À : [log in to unmask]

Objet : [TN] Rigid-Flex PCBA Assembly



Good morning all,



Looks like we'll be getting our hands around a rigid-flex assembly that will need to be produced at our plant in relativity high volume.  I'm referring to PCBA and not the PCB manufacturing.  Although this will be a stimulating challenge that we look forward to, we do not have much experience with this type of board.  Our experience has mainly resided with rigid assemblies.



I'm turning to you this morning in the hopes of getting some direction as how to begin our learning process. Any recommendations on:



- How should we start?



- Do you have any suggested reading?



-Is there training available on this type of assembly process?



-Do you know of any process guru's with a solid experience on PCBA rigid-flex manufacturing that we could contact for guidance?



Any help would be appreciated,



thanks,





EL