I thought he was peeling the copper to check for adhesion to the laminate?
Sent from my iPad Pro
On Tue, Oct 17, 2017 at 9:23 PM +0700, "Ed Popielarski" <[log in to unmask]> wrote:
Hi Victor,
Use this method: http://www.ipc.org/4.0_Knowledge/4.1_Standards/test/2.4.1E.pdf and examine the tape under a 30X microscope. Poor plating issues typically are discovered by observing small pieces of the gold plating (or worse) on the tape.
Regards,
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 360-544-2289
"It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design."
https://goo.gl/maps/mMjg43rXeFB2
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, October 17, 2017 6:53 AM
To: [log in to unmask]
Subject: [TN] Copper Peel Test
Fellow TechNetters:
I have been presented with an opportunity to excel. Has anyone out there conducted a Copper Peel Test om gold fingers on PWB/DIMM/Options cards. The Cu peel test that I am accustom to is on laminate cores. Is this a viable test on very small real estate/surface area.
Victor,
|
|
|