Hi Wayne,
Thanks – helps a lot.
Finish is ENEPIG. Pad size with a perfect etch is 2 mils. Finished copper weight is < 12 microns. Regards Steve
From: Wayne Thayer [mailto:[log in to unmask]]
Sent: August-14-17 11:33 AM
To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly <[log in to unmask]>
Subject: RE: Wire bond wire size versus pad size
Hi Steve-
For the bond pad on the IC, that's the smashed ball size plus targeting error. Smashed balls "normally" are around 3.5 x wire diameter, but using the best tools and equipment I've seen pretty SEM pix down to 1.5 x wire diameter. The bond pad on the IC is beautifully consistent thin film.
For the bond pad on a gold over nickel over copper over laminate board, in "normal" situations you will be placing a "stitch" bond, and added to overall "smashed stitch" plus targeting error, you have the wire potentially wandering beneath the capillary when you're making that second bond. 4 x wire diameter as a minimum dimension is achievable with producible yields. The best gold is electrolytic (not immersion or electroless). If you are working on a single chip package, then all of the nets can be tied together, and you can electrolytically plate the entire structure post-etch. If you have a very complicated, dense route, that isn't possible, so the common technique is to use the electrolytic gold as an etch resist. This leaves "wings" underneath all of the edges. The depth of the wing is dependent on the etching process and the thickness of the copper being etched during the last step. And some etch chemistries preferentially attack nickel, which makes the "wing problem" even worse. Anyway, the "4x" I cited is at the minimum pad cross section, not what was designed or what you see when you look down on the completed etched circuitry.
With the right tools and equipment, you can reverse bond the IC, which improves the targeting on the circuit board and reduces overall bond height at the expense of increased set up and run time. With this technique it is possible to hit 3 x wire diameter minimum cross section bond pads. But then there's another limit I've seen: If you have a fairly thick copper build-up, then ultra narrow bond pads sometimes just break off: The thermosonic process ends up to be too much for the adhesive holding on the original copper plating. The thick copper puts the ultrasonic scrub high enough above this adhesive joint to get a little moment arm on it.
If you're flush with space, double the minimal numbers above and you have enough space for a rework cycle!
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Monday, August 14, 2017 8:03 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Wire bond wire size versus pad size
Hi all,
Is there a general rule of thumb for the wire versus the bond pad size for thermosonic gold wire bonding? Thanks. Steve Kelly
|